Hi all,

I am looking into different wafer cleaning options for diced silicon wafers.
Could somebody advise me with the most usual methods/equipment and their pros
and cons? We need a cheap process for low volume washing. The wafer is mounted
on an adhesive tape.

Thanks,
Markus

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing
MEMStaff Inc.
Addison Engineering