Thermally insulating glue/adhesive
Kirt Williams
2004-10-01
RTV silicones, such as RTV 730, have low thermal conductivities (~0.2
W/m-K).
You squeeze them on and let them cure at room temperature. They are pretty
chemically inert.
    --Kirt Williams

----- Original Message -----
From: "Manscher Martin" 
To: 
Cc: "Manscher Martin" 
Sent: Friday, October 01, 2004 2:41 AM
Subject: [mems-talk] Thermally insulating glue/adhesive


>I was wondering if anyone could recommend a glue/adhesive with low
> thermal conductivity? I have no strong requirements for other
> properties, so any suggestions are welcome.
>
> Martin Manscher, Development Engineer, MSc, PhD
> Danfoss, Microtechnology Group
>
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.memsnet.org/


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Harrick Plasma, Inc.
Process Variations in Microsystems Manufacturing
The Branford Group