MEMSnet Home: MEMS-Talk: Hello! How can I change the hydrophilic PDMS Surfaceto....
Hello! How can I change the hydrophilic PDMS Surfaceto....
2004-10-18
[email protected]
2004-10-20
Bill Moffat
Hello! How can I change the hydrophilic PDMS Surfaceto....
[email protected]
2004-10-18
It has been our experience that the plasma oxidized PDMS suface "recovers" in a
matter of hours without further treatment and returns to being hydrophobic.

--
Jack Rundel
Department of Chemistry
Oregon State University
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
University Wafer
Harrick Plasma, Inc.
Tanner EDA by Mentor Graphics