MEMSnet Home: MEMS-Talk: TiN vs TiW diffusion barrier
TiN vs TiW diffusion barrier
2004-10-19
Thomas Rocco Tsao
2004-10-23
Brad Cantos
TiN vs TiW diffusion barrier
Thomas Rocco Tsao
2004-10-19
As a follow-up to my earlier post on TiN diffusion barriers, I have been
told by one person that TiW is more often used.

Can anybody comment on their experience w/ TiW as a diffusion barrier,
esp how it compares with TiN?

Searching the archives, I can see that basic H2O2 (potentially combined
with EDTA) can be used to etch TiW, but that sometimes, it doesn't work
(i.e. may be some subleties involved).  Does anybody have any personal
experience with etching TiW?

Thanks in advance.

-Tom

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation
Harrick Plasma, Inc.
Tanner EDA by Mentor Graphics