Photoresist does not hold up well to unbuffered HF.  You should use BOE
(HF with NH4F) to pattern SiO2 with resist mask.

Roger Shile

-----Original Message-----
From: [email protected]
[mailto:[email protected]] On Behalf Of Daniel L Baptista
Sent: Thursday, October 28, 2004 1:27 AM
To: [email protected]
Subject: [mems-talk] choosing a good resist

Dear all

I will use a resist on a SiO2 thin layer on a Si substrate. I will
perform
e-beam and single ion lithography to create nanoporous trough the
resist.
Then I need to over-etch the SiO2 layer to produce an undercut. Finally
I
will evaporate metal and lift off the resist. The problem is that using
HF
to etch the SiO2 probably the resist can be affected. My question is
what
resist I should use in this situation. PMMA is good for e-beam but I am
not
sure if it is affected by HF. Could you help me?

Thanks a lot!

Daniel

University of Cambridge, UK
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Process Variations in Microsystems Manufacturing
MEMS Technology Review
Tanner EDA by Mentor Graphics