Dry etch mask
William Lanford-Crick
2004-11-01
Nickel (with Cr or Ti adhesion layer) or NiCr should be good.
-Bill

-----Original Message-----
From: [email protected]
[mailto:[email protected]]On Behalf Of Zhiyan Liu
Sent: Friday, October 29, 2004 5:06 PM
To: [email protected]
Subject: [mems-talk] Dry etch mask


Dear all,

Does anybody has an idea of the dry etch metal mask. The dry etched i used
are Cl2/BCl3.

Thank you ,

Zhiyan

_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics
University Wafer