Dry etch mask
2004-10-29
Zhiyan Liu
2004-11-01
William Lanford-Crick
2004-11-02
Sjoerd Haasl
2004-11-02
William Lanford-Crick
2004-11-22
Zhiyan Liu
Dry etch mask
William Lanford-Crick
2004-11-02
It depends on the power levels and etched time being used for the process.
For long etch times or high power etching, use Ti/Ni, Cr/Ni or NiCr.

-----Original Message-----
From: [email protected]
[mailto:[email protected]]On Behalf Of Sjoerd Haasl
Sent: Tuesday, November 02, 2004 10:03 AM
To: 'General MEMS discussion'
Subject: RE: [mems-talk] Dry etch mask


Hello Zhiyan,

Do you mean what mask to use for dry etching metal?
If so, normal photoresist should work for that. I have used a standard thin
resist (Shipley Megaposit SPR 700-1.2) for etching aluminum with Cl2/BCl3. I
etched 2 microns of aluminum with about 1.5 microns of resist.
Hope this was what you wanted to know.

Sjoerd Haasl

Royal Institute of Technology
Stockholm, Sweden


-----Original Message-----
From: Zhiyan Liu [mailto:[email protected]]
Sent: den 30 oktober 2004 00:06
To: [email protected]
Subject: [mems-talk] Dry etch mask


Dear all,

Does anybody has an idea of the dry etch metal mask. The dry etched i used
are Cl2/BCl3.

Thank you ,

Zhiyan



_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Tanner EDA by Mentor Graphics
University Wafer
Process Variations in Microsystems Manufacturing