A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Carrier for GaAs ECR in BCl3/Cl2
Carrier for GaAs ECR in BCl3/Cl2
2004-11-02
Jobert van Eisden
Carrier for GaAs ECR in BCl3/Cl2
Jobert van Eisden
2004-11-02
Hello all,

I am using 4" Si carriers for Cl2/BCl3 ECR dry etching of 2" GaAs substrates
with AlGaAs/GaAs VCSEL structures. I was wondering if it would be beneficial
to use a few hundred angstroms of Ni on the Si carriers to prevent
suffocation of the process.

Also, I am using a STR 1045 PR mask for the etching process, and have seen
results vary from beautiful to grassy (which is why I consider using a Ni
layer on Si). Does anyone have experience using PR masks for processes like
this? Any input on this would be very welcome.

Thank you in advance,


Jobert van Eisden
College of Nanoscale Science and Engineering
SUNY Albany

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
The Branford Group
Process Variations in Microsystems Manufacturing
University Wafer