MEMSnet Home: MEMS-Talk: Removing PDMS mold from silicon wafer
Source for Si wafers with LPCVD low-stress SiN coating?
2004-11-02
Dong
Removing PDMS mold from silicon wafer
2004-11-03
Aravind
2004-11-03
karim faid
2004-11-03
Jim Beall
2004-11-17
Aravind
Removing PDMS mold from silicon wafer
Aravind
2004-11-03
Hello All,
I am just looking to find out what methods you guys
use to remove the PDMS mold from silicon wafers that
has shapes ethced onto it. I know some people coat the
wafer with HMDS and then pour the PDMS mold over it
and that helps in peeling the PDMS mold off without
any damage to the master..are there any other methods
that work like this? For eg. does anybody have any
experience in coating the wafer with parylene or any
other methods to do this?

Thank you,
Aravind

--- Dong  wrote:

> Hey all,
>
> I am looking for 3" or 4" wafers with 50 to 100 nm
> SiN films on both
> sides.   I will make small tranparent membrane
> windows by wet etching.
> I am looking for rebust, continuous SiN films.
> Anybody know a source
> that provides these wafers?
>
> Please reply to my email address and not to the
> whole groups.  Thanks.
>
> Dongxiang Liao
>
> _______________________________________________
> [email protected] mailing list: to unsubscribe
> or change your list
> options, visit
>
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS
> processing services.
> Visit us at http://www.memsnet.org/
>
>


=====
-------------------------------------------------------------------------------
" Beneath the helmet, under that unruly curly hair, inside the cranium, there is
something we don't know, something beyond scientific measure. Something that
allows him to soar, to roam a territory of sport that, forget us, even those who
are gifted enough to play alongside him cannot even fathom. When he goes out to
bat, people switch on their TV sets and switch off their lives "
-BBC Sports on Sachin Tendulkar
-------------------------------------------------------------------------------



__________________________________
Do you Yahoo!?
Check out the new Yahoo! Front Page.
www.yahoo.com


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
MEMStaff Inc.
Process Variations in Microsystems Manufacturing
The Branford Group