A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Metal Lift-off
Metal Lift-off
2004-11-08
zhiyanl
2004-11-08
Hong Wu
2004-11-08
Isaac Wing Tak Chan
2004-11-09
[email protected]
2004-11-09
Ryoung-han kim
2004-11-09
Tushar Bansal
2004-11-09
William Lanford-Crick
2004-11-09
Shane Jones
2004-11-09
[email protected]
2004-11-09
Bill Moffat
Metal Lift-off
[email protected]
2004-11-09
hi zhiyan..

i had teh same problem a couple of days back.. what was the thicknes of ur
PR.. and what was the thickness of ur metalized layer...

i solved my problem by spinning a thicker layer of PR and having about
500A of metalized layer
regards
karthik

> Dear friends:
>
> I got a trouble when doing metal lift-off with very small feature size. I
> deposited Ti/Au on the patterned PR and then tried to lift off. The
> feature
> size if about 8~10um. But even i soaked it in the acetone for very long
> time,
> the PR still can't be stripped off. It seems the metal not only covered
> the
> top of the PR but also the side wall. I am wondering if you have any idea
> and
> suggestions on how to strip off the PR.
>
> Thank you very much.
>
> Zhiyan
>
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.memsnet.org/
>



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing
The Branford Group
Mentor Graphics Corporation