A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Metal Lift-off
Metal Lift-off
2004-11-08
zhiyanl
2004-11-08
Hong Wu
2004-11-08
Isaac Wing Tak Chan
2004-11-09
[email protected]
2004-11-09
Ryoung-han kim
2004-11-09
Tushar Bansal
2004-11-09
William Lanford-Crick
2004-11-09
Shane Jones
2004-11-09
[email protected]
2004-11-09
Bill Moffat
Metal Lift-off
William Lanford-Crick
2004-11-09
Try ultrasonic agitation.  You need to make sure you have a good sidewall
profile (undercut) to get good liftoff.  Are you doing image reversal?  With
image reversal, the needed undercut profile will be there if you optimize
the process.  Without reversal, you should use a bilayer resist process.

Good luck,
Bill

-----Original Message-----
From: [email protected]
[mailto:[email protected]]On Behalf Of zhiyanl
Sent: Monday, November 08, 2004 11:10 AM
To: General MEMS discussion
Subject: [mems-talk] Metal Lift-off


Dear friends:

I got a trouble when doing metal lift-off with very small feature size. I
deposited Ti/Au on the patterned PR and then tried to lift off. The feature
size if about 8~10um. But even i soaked it in the acetone for very long
time,
the PR still can't be stripped off. It seems the metal not only covered the
top of the PR but also the side wall. I am wondering if you have any idea
and
suggestions on how to strip off the PR.

Thank you very much.

Zhiyan

_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing
The Branford Group