MEMSnet Home: MEMS-Talk: mass spectrometer for RIE end point detection
mass spectrometer for RIE end point detection
2004-11-13
Hoang T Nguyen
2004-11-14
[email protected]
mass spectrometer for RIE end point detection
[email protected]
2004-11-14
Hoang,

Are you using a RIE or an Ion Mill?  You mention both.  There is no beam in
a RIE.  If you are using an RIE "Reactive Ion Etcher" than I have
had very good results using a HeNe reflected off my substrate into a photo
detector connected to a chart recorder.  It is easy to see when you
have milled through one layer of a material and hit another one.

Brent

Original Message:
-----------------
From: Hoang T Nguyen [email protected]
Date: Fri, 12 Nov 2004 16:10:27 -0800
To: [email protected]
Subject: [mems-talk] mass spectrometer for RIE end point detection


Hi,

I am looking for an end point detection method for a reactive ion beam
etching process.  In the process, we have a photoresist mask atop a
SiO2/Hf02 multilayer stack.  We are trying to transfer etch the photoresist
pattern into the SiO2 top layer, but stopping the process once we reach the
HfO2 underlying layer.


Would you recommend a technology to try.

Many thanks,
The ion beam is made up of Ar, O2, and CHF3 plasma.

Hoang Nguyen
Laser Scientist
Lawrence Livermore National Laboratory
[email protected]
408.623.9456
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/

--------------------------------------------------------------------
mail2web - Check your email from the web at
http://mail2web.com/ .


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
The Branford Group
MEMStaff Inc.
Process Variations in Microsystems Manufacturing