[email protected]
PDMS gluing
Lei Wu
2004-11-29
Hi,

I made some channels in the PDMS and punched holes at the end of
channels. Glass slide was bond to PDMS and form the wall of the
channel.Plastic tubes (PEEK tubes)were inserted in the holes and fixed
by various epoxy ester.Solution was pumped into the channels and always
leaked. The glue cannot fast adhere to the PDMS.Can someone give me some
advice on gluing the PDMS and the tubes?


Thanks


Lei
Shenzhen applied R&D centres of city University of Hong Kong
Shenzhen Virtual Univ. Park Room A502, Shenzhen Hi-tech Ind. Park



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Tanner EDA by Mentor Graphics
Harrick Plasma, Inc.
Process Variations in Microsystems Manufacturing