A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: How to clean holes of PI and Mylar films?
How to clean holes of PI and Mylar films?
2004-11-25
oliver77
optimal Al deposition rate on photoresist
2004-11-26
Andrew Xiang
2004-11-26
Isaac Wing Tak Chan
2004-11-26
Andrew Xiang
2004-11-29
Paolo Tassini
2004-11-29
Adrian Brozell
2004-11-29
Michael D Martin
How to clean holes of PI and Mylar films?
Adrian Brozell
2004-11-29
Oliver -

It seems like ultrasonic cleaning would work, but the mylar will float in
solvent.  You are going to have to tie it down.  Five minutes in a Branson
2510 in an ethanol solution should clean the mylar.

Adrian

-----Original Message-----
From: [email protected] [mailto:[email protected]]On
Behalf Of oliver77
Sent: Thursday, November 25, 2004 8:53 AM
To: [email protected]
Subject: [mems-talk] How to clean holes of PI and Mylar films?


Hello

I am looking for a method to clean the holes'  walls  of polyimide and Mylar
films.

The holes was drilled by excimer laser.
The diameters of holes are in 20um~125um.
PI or Mylar film's thickness is 100um.
There are debris , carbine and carbon black sticking on the surface and wall
of holes.
I have tried to clean them with acetone .
But obviously I cannot reach the wall of the holes.

Can ultrasonic cleaning work it out?
How much should be power and frequency of the ultrasonic cleaner ?
Is there any kind of solvent can help to clean them?

Thanks in advance

Oliver Tseng

Project Manager
K-Jet Laser Tek. Inc.
www.kjet.com.tw
Taiwan


_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Mentor Graphics Corporation
Harrick Plasma, Inc.
MEMStaff Inc.