RIE - keep Temp constant
2004-11-30
Karin Buchholz
2004-11-30
Brent Garber
2004-11-30
Shile
2004-11-30
Tripp, Marie Kathleen
2004-11-30
[email protected]
2004-12-01
GRECO Florent
Can vaccum grease be used to bond PDMS to Silica
2004-12-01
Adrian Brozell
2004-12-02
Mohanraj Soundarapandian
RIE - keep Temp constant
Shile
2004-11-30
To provide thermal contact between a substrate and the electrode in an
RIE system, I've used Fomblin grease.  After etch I removed the grease
with Fomblin solvent.

Roger Shile

-----Original Message-----
From: [email protected]
[mailto:[email protected]] On Behalf Of Karin Buchholz
Sent: Monday, November 29, 2004 11:44 PM
To: [email protected]
Subject: [mems-talk] RIE - keep Temp constant

Dear mems talkers,

we have a RIE chamber with temperature control of the 3" carrier wafer.
Since we are just using
 waferpieces we just place these on top of the carrier wafer. It seems
now that these small pieces
 do not have proper thermal contact to the chuck, so the temperature of
the sample is not constant
 from etch to etch and the etch rate also varies by 50per cent...

Do you have any suggestions how to provide good thermal contact? The
manufacturer suggested
Fomblin vaccuum oil, but it is impossible to remove it from the samples
after etching...

I appreciate any help! Have a nice day,

Karin


--
Dipl.-Ing. Karin Buchholz
Walter Schottky Institut
Technische Universitaet Muenchen


_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
University Wafer
Harrick Plasma, Inc.
MEMStaff Inc.