Dear all,

We are using carbon catalyst along with  polymers for
electrode preperation for fuel cells. We use polymer
membranes seperately and in order to stick and
cross-link these polymer membranes with electrodes, we
are trying different methods. Does anyone has similar
experience with this? People worked/ing with carbon,
polymers please suggest me suitable ways for
crosslinking. Also, i would like to know more about
surface chemistry of carbon[activated] when in polymer
mixture.

Thanks for your help,

Venkat.
IMTEK.



__________________________________
Do you Yahoo!?
The all-new My Yahoo! - Get yours free!
http://my.yahoo.com



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
MEMS Technology Review
University Wafer
Tanner EDA by Mentor Graphics