polysilicon molecular weight
2004-12-02
wtt
2004-12-02
David Nemeth
polysilicon molecular weight
David Nemeth
2004-12-02
Polysilicon is not a molecule, and hence has no molecular weight.  It is
many small crystals of silicon, which has an atomic weight of 28.08.

David Nemeth
Senior Engineer
Sophia Wireless, Inc.
14225-C Sullyfield Circle
Chantilly, VA
Ph: (703) 961-9573 x206
Fax:(703) 961-9576

-----Original Message-----
From: [email protected] [mailto:[email protected]]On
Behalf Of wtt
Sent: Thursday, December 02, 2004 10:53 AM
To: [email protected]
Subject: [mems-talk] polysilicon molecular weight


hi

I want to know the
molecular weight of polysilicon
please help me
Thanks

Best regards,

Tina  wen

NTHU, Taiwan






_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/




reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
University Wafer
Process Variations in Microsystems Manufacturing
Harrick Plasma, Inc.