MEMSnet Home: MEMS-Talk: amorphous silicon
amorphous silicon
2004-12-07
li cai
2004-12-07
Isaac Wing Tak Chan
2004-12-07
Paolo Tassini
amorphous silicon
Isaac Wing Tak Chan
2004-12-07
Li,

You can access one of our research group's publication to see that data:

B. Park et al., "Effect of deposition temperature on the structural
properties of n+ mc-Si:H films," Journal of Vacuum Science and Technology
A, vol. 16, no. 2, 1998, pp. 902.


Yours sincerely,

Isaac Chan
University of Waterloo
--------------------------------------------------------------------
My experience is on a-Si:H TFT design and semiconductor processing:
http://resumes.hotjobs.com/iwchan2004/procengineer6yr
--------------------------------------------------------------------

On Mon, 6 Dec 2004, li cai wrote:

> Does anyone know what XRD spectra of amorphous silicon film look like and
> where I can find the information?  Thank you in advance.
>
> Li

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
MEMS Technology Review
Tanner EDA by Mentor Graphics
Mentor Graphics Corporation