A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Bulk Modulus PDMS (in liquid form)
Bulk Modulus PDMS (in liquid form)
2004-12-12
Nathan L. Tyson
2004-12-13
Jeff Zahn
2004-12-13
Wilson, Thomas
Bulk Modulus PDMS (in liquid form)
Jeff Zahn
2004-12-13
A fluid by definition will not have a bulk modulus
since it will deform instantanuously and irreviersibly
when exposed to a shear. It will however, have a
viscosity which determines how much it will deform
when exposed to a shear. If it is viscoelastic it will
have both a storage (elastic) and loss (viscous)
modulus.

--- "Nathan L. Tyson"  wrote:

> Dear Sirs,
>       I am using Gelest PDMS (trimethylsiloxy terminated)
> Silicone Oil (5cSt.)in
> my research and have been unsuccessful in locating
> an estimate (or better
> if possible) of the Bulk Modulus of this oil (not
> crosslinked, but rather
> BM of material in liquid form). I assume that this
> property is temperature
> dependent, and if so, could you give me an idea of
> how radically its value
> varies with temperature? I am using it at 20C and so
> the BM at this temp
> would be most useful. Thanks for your time and
> assistance. I look forward
> to your response.
> Cheers,
> Nathan L. Tyson
> _______________________________________________
> [email protected] mailing list: to unsubscribe
> or change your list
> options, visit
>
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS
> processing services.
> Visit us at http://www.memsnet.org/
>




__________________________________
Do you Yahoo!?
Dress up your holiday email, Hollywood style. Learn more.
http://celebrity.mail.yahoo.com

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
The Branford Group
Tanner EDA by Mentor Graphics
Nano-Master, Inc.