Hi Ning,
We use a tool from Primaxx for our HF vapor release process.  It works
well and the company is very helpful with respect to process and
maintenance help. Their website is:

www.primaxxinc.com

Good luck
Doug



Doug Stewart
Equipment Maintenance Supervisor
Infotonics Corporation
5450 Campus Drive
Canandaigua, NY 14424
(585) 919-3068
[email protected]


-----Original Message-----
From: [email protected]
[mailto:[email protected]] On Behalf Of
[email protected]
Sent: Monday, December 13, 2004 12:02 PM
To: [email protected]
Subject: MEMS-talk Digest, Vol 26, Issue 13

Send MEMS-talk mailing list submissions to
        [email protected]

To subscribe or unsubscribe via the World Wide Web, visit
        http://mail.mems-exchange.org/mailman/listinfo/mems-talk
or, via email, send a message with subject or body 'help' to
        [email protected]

You can reach the person managing the list at
        [email protected]

When replying, please edit your Subject line so it is more specific
than "Re: Contents of MEMS-talk digest..."

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
The Branford Group
Process Variations in Microsystems Manufacturing
Harrick Plasma, Inc.