Sio2 - Sio2 wafer bonding
Brubaker Chad
2004-12-16
Annalisa,

There are a few options which may improve your bonding results.  Since you are
working with oxide surfaces, as you mention, increasing the hydrophilic nature
of the bond process is advantageous.

One method to do that (in a wet chemical manner) is to use a reversed RCA clean
(with no HF dip step).

The process would be:

RCA 2 - HCl:H2O2:H2O 1:1:6, ~70C for ~15 minutes
DI Rinse
RCA 1 - NH4OH:H2O2:H2O 1:1:5, ~70C for ~15 minutes
Di Rinse - Dry

Then, you should actually be able to perform your bonding at room temperature.
You need to be sure that the bonding front is initiated at only one point, so
that you do not get competing bond waves (this will result in a "tenting" effect
where the bond waves meet).

At this point, the bond is very weak.  You should inspect using IR - if you see
significant voids, then separate the wafers, re-activate, and re-bond.  Bear in
mind that, since this bonding relies on Van der Waals forces, it is crucial that
the surfaces are very flat and, more importantly, very smooth (<0.5nm RMA
roughness foe best results).  Then, follow the annealing process you used, and
you should end up with a mostly void free bond.

Regarding plasma, my company as a whole has experience with this, but
unfortunately, I am not allowed to share the details over an open forum.
However, plasma does have the capability to greatly increase both the initial
bond strength and reduce the anneal temperature to full strength (to ~300C).
For further details, you can contact me, or check out the company website at
www.evgroup.com.

Best Regards,
Chad Brubaker

EV Group       invent * innovate * implement
Technology - Tel:  480.727.9635, Fax:  480.727.9700  e-mail:
c.brubaker@EVGroup.com, www.EVGroup.com

This message and any attachments contain confidential or privileged information,
which is intended for the named addressee(s) only. If you have received it in
error, please notify the sender immediately and then delete this e-mail. Please
note that unauthorized review, copying, disclosing, distributing or otherwise
making use of the information is strictly prohibited.

 -----Original Message-----
From:   Annalisa Cerutti [mailto:cerutti@bo.imm.cnr.it]
Sent:   Friday, December 16, 2005 5:38 AM
To:     mems-talk@memsnet.org
Subject:        [mems-talk] Sio2 - Sio2 wafer bonding

Hi,
I want to bond two silicon wafers with thermal oxide (0.5 um) on the
surface.
I tried to bond them in vacuum, with a bonding pressure of 4000 mbar and at
a temperature of 500 °C. Then I performed an annealing at 900 °C for
15
hours. The result was that only small areas bonded.
To improve this result I cannot rise the temperature.
What can I change to improve bonding?
Is O2 plasma activation interesting to hydrophiize the surface?
Do I need a preparation of the surface to hydrophilize it?

Thank's

Annalisa Cerutti

_______________________________________________
MEMS-talk@memsnet.org mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
Addison Engineering
Harrick Plasma, Inc.
Tanner EDA by Mentor Graphics