Vikas:

You can use the CMATRIX macro to calculate the capacitance matrix.  See the
explanation in the "Low-Frequency Electromagnetic Analysis Guide".

Regards,

Dan Shaw
***************************************************



-----Original Message-----
From: [email protected]
[mailto:[email protected]]On Behalf Of Vikas Nair
Sent: Tuesday, December 21, 2004 9:54 AM
To: General MEMS discussion
Subject: [mems-talk] capacitance measurement in ANSYS


Hi,
I am trying to model a comb drive using ANSYS8. I wish to find out the
capacitance of the comb. Can someone please help me out?
Thanks

regards,
Vikas

_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Tanner EDA by Mentor Graphics
Harrick Plasma, Inc.
Mentor Graphics Corporation