A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: How to get rid of the bubbles in the microfluidicdevice.
How to get rid of the bubbles in the microfluidicdevice.
2004-12-31
HAN Anpan
2005-01-04
Manscher Martin
How to get rid of the bubbles in themicrofluidicdevice.
2005-01-05
Danny Klein
Summary. RE: [mems-talk] How to get rid of the bubbles inthemicrofluidicdevice.
2005-01-08
X J
How to get rid of the bubbles in the microfluidicdevice.
HAN Anpan
2004-12-31
Dear Jason

You might try to fill the device with ethanol first and change the reservoir
with what ever buffer. Then use vacuum to remove the ethanol and drag the buffer
into your system. Ethanol have better wetting properties than water. Hope this
helps.

Anpan

-----Original Message-----
From: [email protected] [mailto:[email protected]] On
Behalf Of X J
Sent: mercredi, 22. décembre 2004 18:35
To: [email protected]
Subject: [mems-talk] How to get rid of the bubbles in the microfluidicdevice.


Dear colleagues,
  Hello!
  I work on the microfluidic devices. I found it really annoying that when
I inject the flow there will be always some air bubbles trapped in the
microfluidic devices (made of PDMS and glass). Is there any way to get rid
of them?
  Previously someone recommended to use the ultrasonic toothbrush to tap
the surface of PDMS. But maybe I did not use it correctly, there are still
some bubbles trapped.
  Can I deposit some additional layer to prevent air bubbles from being
trapped?
  For your information,
  The feature size of my device is about 50 um.
  The PDMS is a little bit hydrophobic, long time after treated by oxygen
plasma. And the glass is hydrophilic.

  Thanks a lot!


  Jason


_______________________________________________
[email protected] mailing list: to unsubscribe or change your list options,
visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services. Visit us at
http://www.memsnet.org/



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing
University Wafer