MEMSnet Home: MEMS-Talk: looking for any materials transparent to excimer laser
looking for any materials transparent to excimer laser
2005-01-02
X.Guo
2005-01-03
David Nemeth
looking for any materials transparent to excimer laser
David Nemeth
2005-01-03
David

You might look into MgF2, CaF2, and perhaps even SiO, depending on
thickness.   Check out www.lesker.com for information on possible deposition
methods.  For example, MgF2 is available in sputtering sources.
http://www.lesker.com/newweb/Deposition/Sputter_Targets/ElementNames_J_P/Ma_
magnesiumFluoride.cfm?CFID=581512&CFTOKEN=28963401§ion=magcomps&init=ski
p


David Nemeth
Senior Engineer
Sophia Wireless, Inc.
14225-C Sullyfield Circle
Chantilly, VA
Cell: (202) 288-1067
Ph: (703) 961-9573 x206
Fax:(703) 961-9576

-----Original Message-----
From: [email protected]
[mailto:[email protected]]On Behalf Of X.Guo
Sent: Saturday, January 01, 2005 10:30 PM
To: mems-talk
Subject: [mems-talk] looking for any materials transparent to excimer
laser


Dear all,

Happy the new year!
Does someone know any materials easy to deposit that is transparent to the
excimer laser (such as KrF)?

Thank you very much

Regards,
Xiaojun
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/





reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation
Nano-Master, Inc.
MEMS Technology Review