pink residue film after TiW etching on alumina
2005-01-05
Sarah Higgins
2005-01-05
Pierre Huet
pink residue film after TiW etching on alumina
Sarah Higgins
2005-01-05
The pink film you are seeing is probably gold. It is very common to see
this with this metal system.  It typaclly appears when you heat treat
the the finished substrate.  It can easily be removed using a chemical
etchant.  A dillute Iodine/Potassium Iodine mixture at room temperature
should remove it almost instantly.  A quick dip & rinse should take care
of it.

Sarah Higgins
Palo Alto, CA

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
MEMStaff Inc.
Addison Engineering
Harrick Plasma, Inc.