Sarah Higgins
2005-01-05
Pierre Huet
pink residue film after TiW etching on alumina
Pierre Huet
2005-01-05
This may also be ammonium precipitates. See this link:

http://www.semiconductorfabtech.com/journals/edition.08/download/08.135.
pdf

Regards,
Pierre x286

-----Original Message-----
From: [email protected]
[mailto:[email protected]] On Behalf Of Sarah Higgins
Sent: January 5, 2005 10:09
To: [email protected]
Subject: [mems-talk] pink residue film after TiW etching on alumina

The pink film you are seeing is probably gold. It is very common to see
this with this metal system.  It typaclly appears when you heat treat
the the finished substrate.  It can easily be removed using a chemical
etchant.  A dillute Iodine/Potassium Iodine mixture at room temperature
should remove it almost instantly.  A quick dip & rinse should take care
of it.

Sarah Higgins
Palo Alto, CA
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
MEMStaff Inc.
Harrick Plasma, Inc.
Mentor Graphics Corporation