MEMSnet Home: MEMS-Talk: Ti and Cr resistivity
Ti and Cr resistivity
2005-01-05
Imran Ghauri
2005-01-05
Kirt Williams
2005-01-06
MT Klaus Beschorner
2005-01-07
Damiano Galvan
2005-01-07
MT Klaus Beschorner
Ti and Cr resistivity
Kirt Williams
2005-01-05
See my dissertation, online at
http://www-bsac.eecs.berkeley.edu/archive/kirt_williams_phd.zip,
p. 161, for data on sputtered titanium resistiviy vs. deposition conditions.
I measured 1e-6 to 2.5e-6 ohm-m (not ohm-cm).
    --Kirt Williams

----- Original Message -----
From: "Imran Ghauri" 
To: 
Sent: Wednesday, January 05, 2005 12:05 PM
Subject: [mems-talk] Ti and Cr resistivity


> Hi,
>
> I'm looking for Ti thin film resistiivty and Cr thin
> film resistivity. Resistivity vs. temp. data of these
> thin films will also be appreciated.
>
> Thanks
>
> Imran
> University of Arkansas
>
>
>
>
> __________________________________
> Do you Yahoo!?
> The all-new My Yahoo! - What will yours do?
> http://my.yahoo.com
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.memsnet.org/


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing
MEMStaff Inc.