A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Si02/Si3N4 membranes
Si02/Si3N4 membranes
2005-01-10
[email protected]
2005-01-10
Yanjun Tang
2005-01-10
Michael D Martin
2005-01-10
Altena, G. (Geert)
Si3N4/SiO2 membranes
2005-01-11
[email protected]
2005-01-10
Mattes, Mike
Si02/Si3N4 membranes
[email protected]
2005-01-10
Hi all
I was wondering if someone could help me.
I am trying to etch SiO2/Si3N4 membranes in 100 Si wafer.  The thickness
of the Si3N4 and thermal oxide layers are  100nm
and  2.5micron, respectively.
The Si3N4 layer is removed by the  RIE ,  while  SiO2 in BHF and
then etched in KOH to produce the window membrane. Unfortunately,  each
time I repeat my process the membranes brake.
 Could someone  advise me why this is happening and suggest solution to
this problem.
Also, what are  the best conditions for fabrication of the SiO2 membranes?
Thank you very much in advance.

Maryla


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Addison Engineering
MEMS Technology Review
Process Variations in Microsystems Manufacturing