lift-off
2005-01-11
Li Wang
2005-01-11
Isaac Wing Tak Chan
2005-01-12
Oliver Horn
2005-01-11
Kory Hall
lift-off
Li Wang
2005-01-11
Dear colleague,

I tried to make Ni pattern with lift-off. I used AC for pretty long
time (30 min, 100W, 20 mT). After I immersed the wafer into aceton,
the PR can not be washed away even with Ultrasonic. The PR is
obviously still there because I can see patterns on the PR layer. Can
I use PR stripper instead of aceton? Is stripper compatible with Ni?
I really appreciate if you can share you experience with me. Thank you
very much for help in advance.

Lee

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Tanner EDA by Mentor Graphics
MEMS Technology Review
MEMStaff Inc.