MEMSnet Home: MEMS-Talk: how to coat a large (40inch*50inch) plate
how to coat a large (40inch*50inch) plate
2005-01-10
li xuan
2005-01-10
Gary
2005-01-11
li xuan
2005-01-10
[email protected]
2005-01-11
Brubaker Chad
how to coat a large (40inch*50inch) plate
Brubaker Chad
2005-01-11
Paddy,

One method to coat the large area display is to use a spray coating process.
I've been performing spray coat processing for a while, and have been able to
achieve some pretty impressive results (in some cases, better than (4%
uniformity). The nice thing is, this technology is scalable to pretty much any
size you could desire, and shape of substrate is not a factor. For more
information, please check out the following link:

http://www.micromagazine.com/archive/04/03/brubaker.html

EVG manufactures an ultrasonic spray coating system specifically intended for
large area substrates (designed for large area display systems).

Best Regards,
Chad Brubaker

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Process Variations in Microsystems Manufacturing
MEMS Technology Review
Nano-Master, Inc.