how to etch SiN mask by wet etching?
2005-01-13
NL
2005-01-13
Rana, Mukti M
2005-01-13
Transene
2005-01-13
Isaac Wing Tak Chan
2005-01-13
Kory Hall
2005-01-16
Kirt Williams
how to etch SiN mask by wet etching?
NL
2005-01-13
Dear All,

Generally speaking, SiN mask is patterned by dry etching.But I want to do some
wet etching with SiN mask. At first I sputtered a SiN film on a Si wafer.Then a
standard photolightprocess was processed. Now I don`t know how to etch SiN with
the photoresist.Is the hot phosphoric acid OK?But I`m afraid that the
photoresist can not last for long in the hot phosphoric acid. So what can I do?
Please help me.
Thanks!

LeiNie in HUST of China P.R.
          2005-01-13



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Nano-Master, Inc.
Mentor Graphics Corporation
MEMS Technology Review