Hello everybody,

we have just electrodeposited some Nickel in mold of 2mm length and 30
micrometers think
on some microdevices, have we also made some annealing

we try to do some ebsd analysis on the polished smaples but nothing come out,
even on the annealed one

does someone know a good cleaning receipe for such problems?

thanks
Joe

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation
Nano-Master, Inc.
The Branford Group