how to etch SiN mask by wet etching?
2005-01-13
NL
2005-01-13
Rana, Mukti M
2005-01-13
Transene
2005-01-13
Isaac Wing Tak Chan
2005-01-13
Kory Hall
2005-01-16
Kirt Williams
how to etch SiN mask by wet etching?
Kirt Williams
2005-01-16
HF solutions etch LPCVD Six Ny films only slowly,
but etch most PECVD SiN films, which are lower quality and also have a lot
of hydrogen, rapidly and can therefore be patterned with photoresist.
I'm not sure where sputtered SiN falls in relation to these, but it's worth
trying 5:1 BHF with your sputtered SiN.
    --Kirt Williams

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
MEMStaff Inc.
University Wafer
The Branford Group