Could someone suggest an adhesive for bonding wafers that that can be
patterned and will survive ~24 hr in 25% TMAH at 80degC. The material
should solidified before bond so the wafers can be aligned without
making a mess.

I have used Protek from Brewer Science, but Protek can't be patterned
before etch.  I have also had some success with unexposed SU8, but the
exposed SU8 peels in TMAH.

Roger Shile

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
The Branford Group
Process Variations in Microsystems Manufacturing
MEMS Technology Review