MEMSnet Home: MEMS-Talk: Two metal layer process
Two metal layer process
2005-01-17
Li Wang
2005-01-18
shay kaplan
2005-01-18
David Nemeth
Re: Two metal layer process
2005-01-18
Li Wang
Two metal layer process
David Nemeth
2005-01-18
It sounds like the Al is getting oxidized by air exposure.  You might try
back sputtering, if your system allows it (i.e. sputter the substrate a
little instead of the target to clean off the native oxide.)
You might also look into reworking your design so that both metals can be
deposited without breaking vacuum.  Perhaps there is a selective etch (that
will etch Cr but not Al) that would allow you to expose the Al layer

David Nemeth
Senior Engineer
Sophia Wireless, Inc.

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
MEMS Technology Review
MEMStaff Inc.
Tanner EDA by Mentor Graphics