MEMSnet Home: MEMS-Talk: Recyling test wafers
Recyling test wafers
2005-01-19
Hua Xing Lee
2005-01-20
shay kaplan
Recyling test wafers
shay kaplan
2005-01-20
You can thin them @10u in KOH or if your'e doing CMOS with TMAH.this will
remove the implanted bulk.
Shay