A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Unstable Plasma - Dry Etching
Unstable Plasma - Dry Etching
2005-01-20
William Lanford-Crick
2005-01-20
Isaac Wing Tak Chan
2005-01-21
William Lanford-Crick
2005-01-21
Robert Lindegren
2005-01-21
Frank Torregrosa
HfO2 removal
2005-01-25
rmk111@rsphysse.anu.edu.au
2005-01-20
BobHendu@aol.com
2005-01-21
Capps, Scott
2005-01-25
Blunier, Stefan
Unstable Plasma - Dry Etching
BobHendu@aol.com
2005-01-20
Bill:
Check out the water you are running thru your wafer chuck. Is it controlled by a
chiller unit or house water. You might want to check the resistivity of the
water. Above a certain point it can create what I call thunderbolts in the
chamber. Just replace with distilled water and some ethylene glycol and the
problem should resolve itself. Bob Henderson

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
MEMS Technology Review
Harrick Plasma, Inc.
The Branford Group