Problems with PDMS to PDMS bonding
2005-01-21
Vishwanath Somashekar
2005-01-21
Paul Monaghan
2005-01-21
Z.,W.Y.(Lydia)
Problems with PDMS to PDMS bonding
Z.,W.Y.(Lydia)
2005-01-21
Vishwanath,

1) The purpose of O2 plasma treatment is creating a "wet" surface. You can place
a drop of water on that surface. You should see the water rapidly spread out. If
you have equipment for contact angles measurements, you can monitor this process
better and easiler.

2) If you use Sylgard 184 (Dow Corning), this curing condition is 4 hr at 65C.
Please check your product sheet for detail.

3) If you peel off the PDMS layer from the substrate (especially thin film
<50um) after curing or O2 treatment, it would NOT easy to bond. I have not
figured out why.

4) I did NOT have any problems to bond 2 PDMS layers after O2 plasma treatment.
I just push them together immediately after the O2 treatment.

Good luck,

Lydia

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Nano-Master, Inc.
Mentor Graphics Corporation
Addison Engineering