A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Bonding Kapton to glass
Bonding Kapton to glass
2005-01-25
Joseph P Valentino ([email protected])
2005-01-26
Joseph P. Valentino
2005-01-26
Shay Kaplan
2005-01-26
Bill Moffat
2005-01-26
Joseph P. Valentino
2005-01-26
Michael D Martin
2005-01-26
Brubaker Chad
2005-01-26
Joseph P. Valentino
2005-01-26
[email protected]
Bonding Kapton to glass
Joseph P. Valentino
2005-01-26
I don't know what happened with my original thread but let me try this
again: I'm looking for an adhesive/epoxy that will allow me to permanently
bond sheets of Kapton to glass slides.  I need the adhesive to withstand
temperatures up to 300 deg C and be chemically resistant to most solvents
and acids used in cleanroom processes.  I would prefer it if the adhesive
can be spin-coated on the glass prior to applying the Kapton but this is
not absolutely necessary.  Any ideas?  Thanks,

Joe

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Harrick Plasma, Inc.
The Branford Group
Mentor Graphics Corporation