I sputtered tungsten films over a range of pressures, them measured
thickness and sheet resistance to calculate resistivity.
I also annealed at 900 and 1000 C and remeasured.
All samples were in the range of 15 to 25 micro-ohm-cm, so your value of 20
is just what I'd expect.
    --Kirt Williams