Hello Dhanamjaya

You can use any polymer while isotropic etching of silicon if you use xenon
difluoride. It will not attack your polymers. XACTIX is the overwhelming market
leader in providing equipment for XeF2 silicon etching. If you would like to
try it please give contact me and we can run some samples.

David Springer
XACTIX Inc.
412 381 3195
www.xactix.com

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Addison Engineering
Tanner EDA by Mentor Graphics
The Branford Group