Dear Steve - We have demonstrated microheater elements made from poly-SiC
that operate well above 1100C.  Carbide does not undergo any significant
recrystallization in this temperature range, has stable mechanical
properties, and is therefore well-suited to "take the heat".  Please contact
me offline to discuss further and see if our capabilities can meet your
needs.

        Regards,
         Jeff

__________________
Jeff Melzak
VP of Engineering
FLX Micro, Inc.
Phone: (440)498-4300 x11
Fax: (440)498-4343
[email protected]




reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
MEMS Technology Review
Addison Engineering
Mentor Graphics Corporation