Hi all,

Have any fellow members know where to purchased thick (2mm) wafers high
resistivity Si wafer? These are my specs.

Thanks, Joolien

Details of specification

                Material                                :       HPS
                Orientation                     :       (1-0-0) +/- 1 Deg.
                Type                                    :       P/Bo
                Resistivity     ½ cm    :       > 8,000
                Diameter        mm                      :       100 +/- 0.20
                Flat, Primary   mm              :       SEMI standard
                Flat, Secondary mm              :       SEMI standard
                Thickness                               :       2mm
                Finish                          :       Two side polished
                Edge rounding                   :       Yes, standard
                TTV                                     :       < 3um

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
MEMS Technology Review
MEMStaff Inc.
Mentor Graphics Corporation