Kory Hall
2005-02-14
Hello.  I have a Varian 3125 Sputtering System and I am trying to get a Gold
target for it.  I was told by some target manufacturers that they usually bond
the gold to another base material such as aluminum because the target is so
large and solid gold would be really expensive.  Does anyone know how thick the
layer of gold should be?  Has anyone experienced this before with a sputtering
target?
Thank you,

Kory Hall

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
MEMS Technology Review
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing