Chris Bower
2005-02-18
shay kaplan
2005-02-18
Mark Fuller
Removing epoxy from silicon carbide
Chris Bower
2005-02-18
I have accidentally epoxy bonded a silicon chip to a Silicon carbide (bulk)
tool.  I thought someone on the list might know of a way to selectively
remove the epoxy without damaging the silicon carbide part.  Options that I
have access to are as follows...

High temperature in flowing oxygen?  At some temperature the epoxy should
burn off.  Does anyone know what temperature is safe for the SiC in flowing
oxygen?

Oxygen plasma ashing?  Will the Oxygen plasma touch the SiC?

Wet chemistries? Piranha?

This SiC tool will cost ~$2500 to replace, so I am hoping for some sage
advice :-)

Chris




reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
MEMS Technology Review
MEMStaff Inc.
The Branford Group