Removing epoxy from silicon carbide
2005-02-18
Chris Bower
2005-02-18
shay kaplan
2005-02-18
Mark Fuller
Removing epoxy from silicon carbide
shay kaplan
2005-02-18
Chris,
Most epoxies flow over 150 deg. You can also put both parts into hot resist
strippers. They attack epoxies efficiently
shay