Removing epoxy from silicon carbide
Mark Fuller
2005-02-18
Another solution I've used is MS-111 from miller stephenson.
http://miller-stephenson.com/aero_010.htm

It'll attack all epoxies, dissolving most of them.  It won't dissolve su-8,
but will cause it to swell.

Also, oxygen plasma shouldn't attack SiC.

Mark Fuller
Microelectronics Fabrication Facility
Washington State University

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
MEMS Technology Review
Harrick Plasma, Inc.
University Wafer