MEMSnet Home: MEMS-Talk: Au target Info
Au target Info
2005-02-20
"Alejandro S. Díaz"
Au target Info
"Alejandro S. Díaz"
2005-02-20
We have an old gold sputtering system with a 70 mm targets. It is used
for sample peparation for electron microscope systems, the purity was
not critical, so the backing plates were "refurbished" by a local
goldsmith with a 1 mm layer of .999 gold.

Regards,

                                Sebastian