Badin,

I think but not very sure that Pyrex's thermal conductivity is lower and it
will impact your etch. I only etched through a 50un thin Si wafer bonded to
another thicker (~600um) silicon wafer in Oxford 100 Plasmalab DRIE.

What mask are you going to use?

Good luck,

Hongjun Zeng, PhD

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
Addison Engineering
MEMS Technology Review