MEMSnet Home: MEMS-Talk: protect thin copper film
protect thin copper film
2005-03-03
Xiaoding wei
2005-03-03
Wilson, Thomas
2005-03-03
Pierre Huet
2005-03-03
David Springer
protect thin copper film
David Springer
2005-03-03
Yes as Pierre has suggested XeF2 is a viable option. The attack on copper is
very low or non existent depending on the nature of your device. The XeF2
silicon etch  is a dry gas phase etch so it is very easy to manage. Note that
unlike KOH it is truly isotropic, so the shape of the etch will be different. If
you are interested in how XeF2 might work please give me a call or send me
email. XACTIX is the overwhelming market leader in providing XeF2 etching
equipment so we can even help you try it out if it looks like it makes sense.

Regards
David Springer

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
MEMStaff Inc.
Process Variations in Microsystems Manufacturing
The Branford Group